BS 3473-1

New product

BS 3473-1 91st Edition, July 31, 1991 Chemical Resistance of Glass Used in the Production of Laboratory Glassware Part 1: Method for Determination of Resistance of Glass to Attack by a Boiling Aqueous Solution of Mixed Alkali

More details

$54.80

-60%

$137.00

More info

Description / Abstract: Method and classification for resistance to attack by boiling aqueous sodium carbonate and sodium hydroxide solution.